Austenite Stainless Steel
-
17-7 Steel Strip, Coil, Foil, Wire, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043
● Springs
● Washers
● Clips
●Surgical parts
● Blades
● Bellows
● Honeycomb -
Austenite Stainless Steel
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu N other no greater than 904L 0.02 1 2 0.015 0.03 19~21 24~26 4~5 1~2 - - 253Ma 0.05~0.1 1.4~2 0.8 0.03 0.04 20~22 10~12 - - 0.14~0.2 Ce0.03~0.08 254SMo 0.02 0.8 1 0.01 0.03 19.5~20.5 17.5~18.5 6~6.5 0.5~1 0.18~0.22 - Al-6XN 0.03 1 2 0.03 0.04 20~22 23.5~25.5 6~7 ≤0.75 0.18~... -
Stainless Steel 904L 1.4539
This data sheet applies to stainless steel 904L / 1.4539 hot and cold rolled sheet and strip, semi-finished products, bars, rolled wire and profiles as well as seamless and welded tubes for pressure purposes.